ODREĐIVANJE KARAKTERISTIČNIH MIKROSTRUKTURA ZUT-A KOD SIMULIRANIH I REALNIH SPOJEVA AUSTENITNOG NERĐAJUĆEG ČELIKA 301LN
ODREĐIVANJE KARAKTERISTIČNIH MIKROSTRUKTURA ZUT-A KOD SIMULIRANIH I REALNIH SPOJEVA AUSTENITNOG NERĐAJUĆEG ČELIKA 301LN
/
DETERMINATION OF CHARACTERISTIC MICROSTRUCTURES IN SIMULATED AND REAL HAZ OF 301LN AUSTENITIC STAINLESS STEEL
Oblast / Theme:
NAUKA ISTRAŽIVANJE RAZVOJ/ SCIENCE RESEARCH DEVELOPMENT
Author / Autor-i:
S. Cvetkovski, L. P. Karjalainen